摘要
The aim of this study is to investigate the characteristics of the phase transition for poly(siloxane/ether urethane) copolymers (PSi-EUs) consisting of PTMG/PDMS mixed soft segments and urethane hard segments by differential scanning calorimetry (DSC) and dynamic mechanical analysis (DMA). PSi-EUs exhibit three regions of amorphous phase transition, involving the PDMS soft phase, the PTMG soft phase and the urethane hard phase; therefore, they display phase separation due to low miscibility. Intermolecular hydrogen bonding, which is key to phase mixing, hence resulting in a low degree of phase separation, occurs between the PTMG soft segments in the PTMG/PDMS mixed soft phase and the urethane hard segments. Accordingly, the PSi-EUs are superior to poly(siloxane urethane) copolymer (PSiU) in terms of tensile strength due to the low phase separation and strain-induced crystallization resulting from PTMG soft segments.
原文 | 英語 |
---|---|
頁(從 - 到) | 50-59 |
頁數 | 10 |
期刊 | Polymer Testing |
卷 | 30 |
發行號 | 1 |
DOIs | |
出版狀態 | 已發佈 - 2月 2011 |
ASJC Scopus subject areas
- 有機化學
- 聚合物和塑料