Atomic layer deposition-based functionalization of materials for medical and environmental health applications

Roger J. Narayan, Shashishekar P. Adiga, Michael J. Pellin, Larry A. Curtiss, Alexander J. Hryn, Shane Stafslien, Bret Chisholm, Chun Che Shih, Chun Ming Shih, Shing Jong Lin, Yea Yang Su, Chunming Jin, Junping Zhang, Nancy A. Monteiro-Riviere, Jeffrey W. Elam

研究成果: 雜誌貢獻文章同行評審

47 引文 斯高帕斯(Scopus)

摘要

Nanoporous alumina membranes exhibit high pore densities, well-controlled and uniform pore sizes, as well as straight pores. Owing to these unusual properties, nanoporous alumina membranes are currently being considered for use in implantable sensor membranes and water purification membranes. Atomic layer deposition is a thin-film growth process that may be used to modify the pore size in a nanoporous alumina membrane while retaining a narrow pore distribution. In addition, films deposited by means of atomic layer deposition may impart improved biological functionality to nanoporous alumina membranes. In this study, zinc oxide coatings and platinum coatings were deposited on nanoporous alumina membranes by means of atomic layer deposition. PEGylated nanoporous alumina membranes were prepared by self-assembly of 1-mercaptoundec-11-yl hexa(ethylene glycol) on platinum-coated nanoporous alumina membranes. The pores of the PEGylated nanoporous alumina membranes remainedfree of fouling after exposure to human platelet-rich plasma; protein adsorption, fibrin networks and platelet aggregation were not observed on the coated membrane surface. Zinc oxide-coated nanoporous alumina membranes demonstrated activity against two waterborne pathogens, Escherichia coli and Staphylococcus aureus. The results of this work indicate that nanoporous alumina membranes may be modified using atomic layer deposition for use in a variety of medical and environmental health applications.
原文英語
頁(從 - 到)2033-2064
頁數32
期刊Philosophical Transactions of the Royal Society A: Mathematical, Physical and Engineering Sciences
368
發行號1917
DOIs
出版狀態已發佈 - 4月 28 2010

ASJC Scopus subject areas

  • 一般數學
  • 一般工程
  • 一般物理與天文學

指紋

深入研究「Atomic layer deposition-based functionalization of materials for medical and environmental health applications」主題。共同形成了獨特的指紋。

引用此