TY - JOUR
T1 - Influence of handheld nonthermal plasma on shear bond strength of polyaryletherketone to resin-matrix cement
AU - Huang, Huei Yu
AU - Lai, Szu Yu
AU - Lee, Fu Ting
AU - Wu, Yang Che
AU - Feng, Sheng Wei
AU - Nikawa, Hiroki
AU - Peng, Tzu Yu
N1 - Publisher Copyright:
© 2024 Association for Dental Sciences of the Republic of China
PY - 2024/10
Y1 - 2024/10
N2 - Background/purpose: Challenges exist regarding the bonding efficiency of polyaryletherketone (PAEK), a high-performance thermoplastic, attributed to its chemical inertness and hydrophobic surface, hindering effective bonding with resin-matrix cement. This research explored the impact of handheld nonthermal plasma (HNP), under varying operational parameters, on PAEK surface wettability and changes in bonding performance with cement. Materials and methods: Three types of disc-shaped PEAK specimens were prepared, with surface treatments categorized as grinding, airborne-particle abrasion (APB), and HNP. Surface wettability was analyzed using a contact angle analyzer (n = 10). Specimens were bonded with resin cement and subjected to artificial aging tests: distilled water bath (NA), thermocycling, and highly accelerated stress tests (n = 10 for each test). Shear bond strength (SBS) was measured, failure modes were analyzed, and statistical analyses were conducted. Results: The HNP markedly improved PAEK surface wettability, achieving superhydrophilicity (P < 0.05). This effect intensified with extended operation times (30 or 60 s) and reduced elapsed times (<30 s). HNP-treated PAEK exhibited higher SBS than APB (P < 0.05) and maintained bonding durability after artificial aging, particularly in ketone-enriched variants. Failure analysis revealed predominantly adhesive failure under APB–NA treatment, mixture failures under HNP–NA treatment and postaging, but no cohesive failure. Conclusion: The HNP device benefits dental settings by transforming the PAEK surface into superhydrophilic properties, thereby improving PAEK–cement bonding. It significantly enhances bond durability within 30 s of operation and after a 30 s elapsed period. It is noteworthy that ketone-enriched PAEK demonstrates markedly improved bonding performance.
AB - Background/purpose: Challenges exist regarding the bonding efficiency of polyaryletherketone (PAEK), a high-performance thermoplastic, attributed to its chemical inertness and hydrophobic surface, hindering effective bonding with resin-matrix cement. This research explored the impact of handheld nonthermal plasma (HNP), under varying operational parameters, on PAEK surface wettability and changes in bonding performance with cement. Materials and methods: Three types of disc-shaped PEAK specimens were prepared, with surface treatments categorized as grinding, airborne-particle abrasion (APB), and HNP. Surface wettability was analyzed using a contact angle analyzer (n = 10). Specimens were bonded with resin cement and subjected to artificial aging tests: distilled water bath (NA), thermocycling, and highly accelerated stress tests (n = 10 for each test). Shear bond strength (SBS) was measured, failure modes were analyzed, and statistical analyses were conducted. Results: The HNP markedly improved PAEK surface wettability, achieving superhydrophilicity (P < 0.05). This effect intensified with extended operation times (30 or 60 s) and reduced elapsed times (<30 s). HNP-treated PAEK exhibited higher SBS than APB (P < 0.05) and maintained bonding durability after artificial aging, particularly in ketone-enriched variants. Failure analysis revealed predominantly adhesive failure under APB–NA treatment, mixture failures under HNP–NA treatment and postaging, but no cohesive failure. Conclusion: The HNP device benefits dental settings by transforming the PAEK surface into superhydrophilic properties, thereby improving PAEK–cement bonding. It significantly enhances bond durability within 30 s of operation and after a 30 s elapsed period. It is noteworthy that ketone-enriched PAEK demonstrates markedly improved bonding performance.
KW - Highly accelerated stress aging tests
KW - Nonthermal plasma
KW - Polyaryletherketone
KW - Resin-matrix cement
KW - Shear bond strength
KW - Superhydrophilic
UR - http://www.scopus.com/inward/record.url?scp=85195093925&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=85195093925&partnerID=8YFLogxK
UR - https://www.mendeley.com/catalogue/cddc82ca-86e0-345c-a440-725a0a1678f5/
U2 - 10.1016/j.jds.2024.05.029
DO - 10.1016/j.jds.2024.05.029
M3 - Article
C2 - 39347046
AN - SCOPUS:85195093925
SN - 1991-7902
VL - 19
SP - 2057
EP - 2064
JO - Journal of Dental Sciences
JF - Journal of Dental Sciences
IS - 4
ER -